Minerals – Ceramic Action
The trick was to fire the kiln normally and then cool the kiln very rapidly to about 1000C which is the stage in which the viscous molten material starts to harden and then hold the kiln at a steady temperature in a reduced oxygen environment for an hour or two then begin a very slow 2 degree per minute drop in the same reduced oxygen environment until the glaze had completely solidified around